研究了钛酸钡和钛酸钙担载的Ag和Pt纳米催化剂的表面结构随氧化-还原处理过程的动态变化及其对CO完全氧化反应性能的影响.发现氧化物担载的Ag催化剂在氧化处理后其催化活性较还原处理的高;X射线衍射(XRD)和X射线光电子能谱(XPS)表征结果表明,氧化处理能够提高载体表面Ag颗粒的分散度,而还原处理导致Ag颗粒的聚集,从而降低了催化氧化CO反应的活性.氧化-还原处理改变了担载Ag纳米粒子的尺寸并影响其CO氧化反应活性.与此相反,氧化物担载的Pt催化剂在还原处理后所表现出的CO氧化反应活性较氧化处理的高;对比研究发现,氧化和还原处理后Pt纳米粒子的尺寸基本相同,但是氧化处理的样品中Pt表面物种以氧化态为主,而还原处理后Pt表面物种主要为金属态.Pt纳米粒子表面化学状态随氧化-还原处理的调变是导致表面催化活性差异的主要原因.

参考文献

[1] Dissanayake D;Kharas K C C;Lunsford J H;Rosynek M P .[J].Journal of Catalysis,1993,139:652.
[2] Kremenic G;Nieto J M L;Tascon J M D;Tejuca L G .[J].J Chem Soc Faraday Trans 1,1985,81:939.
[3] Shu J;Kaliaguine S .[J].Applied Catalysis B:Environmental,1998,16:L303.
[4] Nishihata Y;Mizuki J;Akao T;Tanaka H Uenishi M Kimura M Okamoto T Hamada N .[J].NATURE,2002,418:164.
[5] Uenishi M;Taniguchi M;Tanaka H;Kimura M;Nishihata Y;Mizuki J;Kobayashi T .Redox behavior of palladium at start-up in the Perovskite-type LaFePdOx automotive catalysts showing a self-regenerative function[J].Applied Catalysis, B. Environmental: An International Journal Devoted to Catalytic Science and Its Applications,2005(4):267-273.
[6] Lee Y L;Kleis J;Rossmeisl J;Morgan D .[J].Physical Review B:Condensed Matter,2009,80:224101/1.
[7] Orikasa Y;Ina T;Nakao T;Mineshige A Amezawa K Oishi M Arai H Ogumi Z Uchimoto Y .[J].Physical Chemistry Chemical Physics,2011,37:16637.
[8] Costa C N;Sawa P G;Andronikou C;Lambrou P S Polychronopoulou K Belessi V C Stathopoulos V N Pomonis P J Efstathiou A M .[J].Journal of Catalysis,2002,209:456.
[9] Costa C N;Stathopoulos V N;Belessi V C;Efstathiou A M .[J].Journal of Catalysis,2001,197:350.
[10] Machocki A;Ioannides T;Stasinska B;Gac W;Avgouropoulos G;Delimaris D;Grzegorczyk W;Pasieczna S .Manganese-lanthanum oxides modified with silver for the catalytic combustion of methane[J].Journal of Catalysis,2004(2):282-296.
[11] Giebeler L;Kiessling D;Wendt G .LaMnO3 perovskite supported noble metal catalysts for the total oxidation of methane[J].Chemical Engineering & Technology: Industrial Chemistry -Plant Equipment -Process Engineering -Biotechnology,2007(7):889-894.
[12] Cimino S;Lisi L;Pirone R;Russo G .[J].Industrial and Engineering Chemistry Research,2004,43:6670.
[13] Mu R T;Guo X G;Fu Q;Bao X H .[J].J Phys Chem C,2011,115:20590.
[14] Mu R T;Fu Q;Liu H Y;Tan D L Zhai R Sh Bao X H .[J].Applied Surface Sinence,2009,255:7296.
[15] Singh U G;Li J;Bennett J W;Rappe A M Seshadri R Scott S L .[J].Journal of Catalysis,2007,249:349.
[16] Li, J;Singh, UG;Bennett, JW;Page, K;Weaver, JC;Zhang, JP;Proffen, T;Rappe, AM;Scott, S;Seshadri, R .BaCe1-xPdxO3-delta (0 <= x <= 0.1): Redox Controlled Ingress and Egress of Palladium in a Perovskite[J].Chemistry of Materials,2007(6):1418-1426.
[17] Radonjic L;Todorovic M;Miladinovic J .[J].JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY,2008,45:125.
[18] Zhang H J;Chen G;Li Y X;Teng Y J .[J].International Journal of Hydrogen Energy,2010,35:2713.
[19] Mu R T;Fu Q;Xu H;Zhang H Huang Y Y Jiang Zh Zhang Sh Tan D L Bao X H .[J].Journal of the American Chemical Society,2011,133:1978h.
[20] Qu Zh P;Huang W X;Cheng M J;Bao X H .[J].Journal of Physical Chemistry B,2005,109:15842.
[21] Wang W;Zhang H B;Lin G D;Xiong Zh T .[J].Applied Catalysis B:Environmental,2000,24:219.
[22] Pecchi G;Campos C M;Jiliberto M G;Fierro J L G .[J].Applied Catalysis A:General,2009,371:78.
[23] Rajesh T;Rajarajan A K;Gopinath C S;Devi R N .[J].J Phys Chem C,2012,116:9526.
[24] Dacquin J P;Lancelot C;Dujardin C;Cordier-Robert C Granger P .[J].J Phys Chem C,2011,115:1911.
[25] Fabbrini L;Kryukov A;Cappelli S;Chiarello GL;Rossetti I;Oliva C;Forni L .Sr1-xAgxTiO3 +/-delta (x=0, 0.1) perovskite-structured catalysts for the flameless combustion of methane[J].Journal of Catalysis,2005(2):247-256.
[26] Buchneva O;Rossetti I;Biffi C;Allieta M Kryukov A Lebedeva N .[J].Applied Catalysis A:General,2009,370:24.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%